Contact Us
HOME >Case Studies> SUGAR PLANTS

Hardfacing Of Static Coller

Industry Type
Sugar

Product Group
Electrode

OUR SOLUTION

Polarity
+VE

Power Source
Rectifier

Process
SMAW

Quantity (Kgs)
10

Current (amps)
120

Size (mm)
4.00

Product
Lotherme -605

JOB PICTURES
Job Sketch With Dimension

Job Sketch With Dimension

ANALYSIS

Dimensions (Mm)
20

Comp. Weight (Kgs)
300 Kg

Base Metal
SS Liner Fitted Over Mild Steel

Previous Solution
Rebuild With E124(Ador) And No Hardfacing

Problem Due To
Metal To Metal Wear And Compressive Load

Type Of Problem
Frictional Wear

Component Name
Static Coller

Equipment Name
Roller Side Static Coller

1. Remove the fatigue metal.

2. Clean the surface from grease and dust

3. Weld the wear out area with loth-605, 4.00 mm, is used to resist the metal to metal wear.

4. Grind the surface upto level of surface.

Further Reading on Case Studies

Leveler Blade Reconditioning
Read Case Study
Raw Juice Pump Casing Reconditioning
Read Case Study
Teeth Of Sprocket
Read Case Study