Cast Iron welding

Industry Type

Product Group

ANALYSIS

DIMENSIONS (mm) T * D
90*450

BASE METAL
CAST IRON

PREVIOUS SOLUTION
Welding with Ferroloid 1 (Esab welding Rod)

PROBLEM DUE TO
Improper Manufacturing

TYPE OF PROBLEM
Defects as Blow holes in part

COMPONENT NAME
Manufacturing Defects

EQUIPMENT
C.I. Wheels

JOB PICTURES

Cast Iron Job

Cast Iron Job

Our solution

Qty. (Kgs)
16

Current (AMPs)
125

Size (mm)
3.15

Product
LOTHERME 703

Procedure

PROCEDURE :

*CLEANED WELD AREA FREE OF CONTAMINATION, OIL, GREASE, DUST.

*REMOVED THE ENTIRE DEFECTED AREA BY GRINDING.

*FILLING UP THE GAP BETWEEN IT BY WELDING OF LOTHERME 703.

Further Reading on Case Studies