Filling the Defects in Casting by Welding Rods

Industry Type

Product Group

ANALYSIS

DIMENSIONS (mm) L * T * W
2.4*0.6*1

COMP. WEIGHT (kgs)
5 Tonnes

BASE METAL
Cast Iron

PREVIOUS SOLUTION
L &T CPCI 026

PROBLEM DUE TO
Manufacturing Process

TYPE OF PROBLEM
Defects in casting

COMPONENT NAME
Press Dies

EQUIPMENT
Cast Iron Job

JOB PICTURES

Cast Iron Job

Cast Iron Job

Our solution

Qty. (Kgs)
10kgs

Current (AMPs)
110Amps

Size (mm)
3.15

Product
Lotherme 703

Procedure

1. Electrodes are baked to 250 deg C for 1hour.

2. Surface to be welded is cleaned.

3. Defects are filled with Lotherme 703 at 110Amps of current .

4. Excess welding is finished with the help of grinder.