MDF shaft reconditioning in furnace

Industry Type

Product Group

ANALYSIS

DIMENSIONS (MM) L x Outer Dia
3000Lx 200Dia

PROBLEM
Wear

WEAR FACTOR
Temp, abrasion

TEMP (Deg.C)
750-800

MODEL
na

MATERIAL HANDLED
Molten Iron

BASE METAL
15Mo3

EQUIPMENT
Furnace

Job Pictures

before

before

after

after

Our Solution

QTY (Kgs)
40kg

Size (mm)
2.4mm

Product
LothermeGS 602

Procedure

-Clean area of shaft surface and removing hook from shaft as mentioned in below picture.

-Pre heat the job 250deg before welding

-Follow GMAW process using Our Product LoTherme GS602 and maintain inerpass temp.

-Build up on shaft to its original dimension

-Slow cooling required after welding.

-Machining