Get the product details over an email

1. Ensure the electrodes are dry. Re-dry the electrodes at 250°C for one hour.
2. When welding on high hardenable materials of large thicknesses, adequate care for preheating, slow cooling & PWHT are necessary.
3. Use short arc & minimum weaving.
Element | C | Mn | Si | Cr | Ni | Mo | V |
Percent | 0.09 | 1.55 | 0.45 | 2.80 | 2.25 | 1.20 | 0.30 |
After SR 560°C for one hour: 36-39 RC
Size (mm) Dia x Length | 8x450 | 6.3x450 | 5x450 | 4x450 |
Current Range (Amps) | 300-350 | 250-280 | 200-250 | 150-180 |
Weight / Carton (kgs) | 5 | 5 | 5 | 5 |