REBUILDING OF MANDREL

Industry Type

Product Group

ANALYSIS

BASE METAL
+HF

PREVIOUS SOLUTION
ADORLH717/ L&TEUT 6800

PROBLEM DUE TO
IMPACT/ TEM PERATURE

NATURE OF PROBLEM
METAL TO METAL WEAR

PROBLEM
METAL TO METAL WEAR WHILE M AKING SEAM LESS PIPE M ANDRILL GETSWORN OUT BECAUSE OF HIGH TEM P. 900* C. WE ARE GETTING 250-300 SHOTS PER M ANDRILL.

PRODUCT DETAIL
MANDREL

Job Pictures

REBUILDING OF MANDREL

REBUILDING OF MANDREL

Our Solution

QTY (Kgs)
10KG/ PER JOB

Size (mm)
3.15

Product
LOTHERME-514

Procedure

TYPE OF WEAR: IMPACT

WORKING TEM PERATURE: 900 DEGREE


LoTherme-514 is ideally suited for welding Ni-Cr-Mo alloys to themselves, to other metals and for surfacing steel with Ni-Cr-Mo deposit. Applications in this category include valves, pumps, etc. 

Further Reading on Case Studies

WELDING REBUILDING OF RING ROLLING CO-AXIAL ROLL

Read Case Study

Hard Facing Of The Nozzle Tip

Read Case Study
Contact Us