CNM (SPL) is a special formulated electrode to deposit a very high strength weld metal. The weld metal possesses high strength and toughness and is ideally suited for welding high strength steels.
1. Ensure the electrodes are dry. Re-dry the electrodes at 300°C for 2 hours.
2. Use short arc and stringer beads.
3. Use a carefully formulated welding procedure with preheat and post weld heat treatment.
Element | C | Mn | Si | Cr | Ni | Mo | S | P |
Percent | 0.07 | 1.0 | 0.35 | 1.0 | 2.2 | 0.95 | 0.025 | 0.025 |
UTS | YS | Elongation | CVN Impact Strength (J) |
(MPa) | (MPa) | (L= 5d)% | at 0°C |
970 | 861 | 16.0 | 50 |
Size (mm) | 6.3x450 | 5x450 | 4x450 | 3.15x450 | 2.5x350 |
Current Range (Amps) | 270-320 | 200-250 | 150-190 | 100-140 | 60-90 |
Qty. (Pcs./Carton) | 25 | 35 | 55 | 75 | 125 |