Get the product details over an email

It is a rutile coated electrode yielding an extra low carbon (0.025% max) with ferrite (6 -12 FN) in the weld metal. The weld metal has excellent resistance to intergranular corrosion even at elevated temperatures.
1. Ensure the electrodes are dry. Re-dry the electrodes at 250-300°C for one hour.
2 Use lowest size of electrode possible and low current.
3 Use short arc.
Element | C | Mn | Si | S | P | Cr | Ni | Mo |
Percent | 0.021 | 1.75 | 0.30 | 0.020 | 0.022 | 19.0 | 12.0 | 2.4 |
UTS | Elongation |
(MPa) | (L= 4d)% |
535 | 38.0 |
Size (mm) | 5x350 | 4x350 | 3.15x350 | 2.5x350 |
Current Range (Amps) | 150-180 | 110-140 | 80-100 | 60-80 |
Weight / Carton (kgs) | 2.5 | 2.5 | 2.5 | 2.5 |